PVDF (Polyvinylidene fluoride ) binder is for mixing together with cathode powder to prepare Li-ion battery
electrode 80g/bag, vacuum sealed in the plastic bag
SPECIFICATIONS:
Technical Parameter | Unit | Index | Testing |
Shape | / | White Powder | / |
Purity | % | ≥99.5 | PVDF |
standard specific gravity | / | 1.74~1.77 | ASTM D 792 @23/ 23℃ |
Dielectric constant | 100MHz | 4.50~5.50 | ASTM D150 |
Melting Point | ℃ | 160-168 | ASTM D 3418 |
Melting Index | g/10min | 1-2 | / |
Solubility | / | Transparent and dissolvable | 30℃,1hr 1g/10ml NMP |
Rotation Viscosity | mPa·S | ≥2000 | 1g/10ml NMP, 30℃ |
Intrinsic Viscosity | dL/g | 1.0-2.0 | DMA, 30℃ |
Moisture | % | ≤ 0.1 | Karl Fischer |
Molecular Weight | / | 600,000 | ASTM D 5296-05 |
Application Notes: Please click to see Step by Step Recipe for Preparing Anode & Cathode Electrode Slurry
Note:
PVDF resins have good thermostability at the temperature below 310℃. However, it will decompose into the toxic
hydrogen fluoride and fluorocarbon if it is idle for a long time at the temperature between 310~ 320℃. It is not suggested
to use PVDF resin at temperature higher than 370℃ because this will accelerate the decomposition velocity in such
an environment. Besides, please keep in mind that PVDF resin will release toxic hydrogen fluoride and fluorocarbon when it burns.