Phone(+65) 6284 3818 | sales@premier-sols.com | Enquriy |
Aiming to replace of the traditional PVDF binder, this non-toxic polymer binder (Polyolefin grafted acrylic acid copolymer) for Li-ion cathode features strong electrolyte
resistance and high viscosity, and one of the advantage from water-based (Aqueous) chemistry is it isn't prone to catching fire.
Mixing guide:
1. 3.0% in weight (for customer's reference) of the mixing powder (active+conductive+binder), no thicken agent required
2. Put mixed powder into ball milling machine to dry mill.
3. Add water as solvent for paste mixing.
4. Add Alcohol to prevent bubble and aging for 4-8 hours
5. Vacuum mixing for 10-20 minutes for use.
Sepecification:
Apperance: White powder
Viscosity: 200~300mpa.s
PH: 6~8
Purity: ≥99%
Ash: ≤0.3%
Storage and Handling:
Powder in bottle covered by vacuum Al bag
Non-harzard product
1 year shelf life if under 38℃
Application Notes:
Please click to see Step by Step Recipe for Preparing Anode & Cathode Electrode Slurry